Wafer #240918-24 – 1 μm Microslit – Gold Coated
Manufacturer’s Data
- Logged by: Ahmet Gurcan
- Membrane Type: MSSN 1 micron Microslit – Gold Coated
- SKU: MSSN400.C-3LX.1-1.0E2-AU
- Lot Number: 240918-24
- Quantity Received: 200
- Manufacturer Test Report:
- Flow Data Avg in SLPM
- 4psi: 4.5
- 15psi: 10.58
- Burst: 66.78 PSI
- Flow Data Avg in SLPM