| Nanoparticles Inventory – taken by Karl on 11/2/12. All these particles can be found in the refrigerator. | |||||
| Manufacturer | size | type | amount (approx) | expiration date | fluorescence (if applicable) |
| BBI | 5nm | gold colloid | 3mL | Jan-10 | |
| BBI | 5nm | gold colloid | 6mL | Aug-11 | |
| BBI | 10nm | gold colloid | 2mL | Jun-11 | |
| BBI | 10nm | gold colloid | 2mL | May-09 | |
| BBI | 15nm | gold colloid | 2mL | Oct-09 | |
| BBI | 15nm | gold colloid | 20mL | Feb-13 | |
| BBI | 20nm | gold colloid | 20mL | Jun-13 | |
| BBI | 30nm | gold colloid | 15mL | Feb-11 | |
| BBI | 40nm | gold colloid | 5mL | Dec-09 | |
| BBI | 40nm | gold colloid | 20mL | Jun-11 | |
| SPI | 2nm | gold colloid | 100mL | Mar-08 | |
| SPI | 5nm | gold colloid | 100mL | Dec-07 | |
| SPI | 10nm | gold colloid | 100mL | Jan-08 | |
| Invitrogen | 0.02um | Q-dot carboxy fluorospheres | 10mL | not given | 580/605 |
| Invitrogen | 0.05um | Q-dot carboxy fluorospheres | 1mL | not given | |
| Invitrogen | 0.02um | Q-dot carboxy fluorospheres | 4mL | not given | 505/515 |
| Invitrogen | 0.1um | Q-dot carboxy fluorospheres | 8mL | not given | 505/515 |
| Invitrogen | 0.04um | Q-dot carboxy fluorospheres | 1mL | not given | 505/516 |
| Invitrogen | 0.02um | flurosphere size kit carboxy-modified microspheres | 1mL | not given | 505/517 |
| Invitrogen | 0.1um | flurosphere size kit carboxy-modified microspheres | 1mL | not given | 505/518 |
| Invitrogen | 0.2um | flurosphere size kit carboxy-modified microspheres | 1mL | not given | 505/519 |
| Invitrogen | 1um | flurosphere size kit carboxy-modified microspheres | 1mL | not given | 505/520 |
| Invitrogen | 2um | flurosphere size kit carboxy-modified microspheres | 1mL | not given | 505/521 |
| Avanti | carboxy-functionalized | 500uL | not given | 498/515 | |
| Avanti | amine-functionalized | 500uL | not given | 498/516 | |
| Avanti | non-functionalized | 500uL | not given | 498/517 | |
| Bangs Laboratory | 0.15um | acylic polymer uniform dyed microspheres | 5mL | Jan-00 | |
| Bangs Laboratory | 0.97um | silica uniform dyed microspheres | 1mL | Jan-00 | |
| Bangs Laboratory | 1.04um | P(S/V-COOH) | 2mL | Jan-00 | |
| Polysciences | 3um | polybead carboxylate microspheres | |||
| Polysciences | 45um | polybead polystyrene latex beads | 2mL | not given | |
| G Kisker | 1um | silica, plain | 5mL | not given | |
| G Kisker | 1um | silica, COOH functionalized | 5mL | not given | |
| G Kisker | 200nm | red silica, plain | 5mL | not given | |
| G Kisker | 200nm | red silica, COOH functionalized | 5mL | not given | |
| ALSO: ~15 bottles of assorted nanoparticles with moldy labels and precipitated particles | |||||
| 2 Invitrogen Q-dot 655 antibody conjugation kits | |||||