Wafer #1523 – 1 Slot NPN

Manufacturer’s Data

  • Delivery Date: 2/28/2024 (picked up and logged by Ahmet Gurcan)
  • Membrane Type:  NPN 1 Slot
  • SKU: NPSN100-1L-TE
  • Lot Number: 1523
  • Quantity Received: 237
  • Manufacturer Test Report:
    • Pore Size: 52.7nm
      Porosity: 15.0%
      Flow Data Avg in SLPM
      2psi: 0.126
      4psi: 0.276
      Burst: 6.151
  • Packing slip & invoice: None

UR Testing

 

Experiences

  • Cell culture
    • Lananh is having issues with cell culture as of 3/25/2024 with this lot
      • The issue was not with the lot, but rather the cells (4/15/2023).