Wafer #1526 – 1 Slot NPN
Manufacturer’s Data
- Delivery Date: 2/28/2024 (picked up and logged by Ahmet Gurcan)
- Membrane Type: NPN 1 Slot
- SKU: NPSN100-1L-TE
- Lot Number: 1526
- Quantity Received: 211
- Manufacturer Test Report:
- Pore Size: 49.2nm
- Porosity: 15.5%
- Flow Data Avg in SLPM
- 2psi: 0.130
- 4psi: 0.248
- Burst: 5.510
- Packing slip & invoice: None
UR Testing
- Porosity: N/A
- Pore size: N/A
- Pore morphology: N/A
- EDS: N/A
- Chip and Membrane Appearance – (Box Folder: https://rochester.box.com/s/0vk3m9erbkyo2pbrdq6okdk3de90q713 ).
- Membrane dimensions (flat surface): 0.7 mm x 2 mm
- Representative membrane Image: See Below.

Experiences
- Cell culture (none as of 2/28/2024)