Wafer #1525 – 1 Slot NPN

Manufacturer’s Data

UR Testing

  • Porosity: 12.5 +/- 0.95%
  • Pore size: 59.5 +/- 1.5 nm
  • Pore morphology: 0.86 +/- 0.02 circularity
  • EDS: N/A
  • 3 Membranes from this lot were removed for QC measurments
  • Chip and Membrane Appearance – (Box-Folder: https://rochester.box.com/s/inrx2wktj6hejlm5h7eifrvzwy7lilhc).
  • Membrane dimensions (flat surface): 0.7 mm x 2 mm
  • Representative membrane Image: See Below.

Experiences

  • Cell culture (none as of 6/20/2024)