Wafer #240803-09 – 2 Slot NPN
Manufacturer’s Data
- Delivery Date: 12/18/2024 (picked up and logged by Ahmet Gurcan)
- Membrane Type: NPN 2 Slot
- SKU: NPSN100-2LWMS
- Lot Number: 240803-09
- Quantity Received: 20
- Manufacturer Test Report:
- Pore Size: 51.8 nm
- Porosity: 13.5%
- Flow Data Avg in SLPM
- 2psi: 0.304
- 4psi: 0.584
- Burst: 4.882
UR Testing
- Porosity: 11.72%
- Pore size: 52.42 +/- 15.33 nm
- Pore morphology: Standard
- EDS: N/A
- 3 Membranes from this lot were removed for QC measurements.
- Chip and Membrane Appearance – (Box-Folder: https://rochester.box.com/s/fta416emzuaoe4gezs08bq4qpc3vxoz9 ).
- Membrane dimensions (flat surface): 2 x (0.7 mm x 2 mm)
- Representative membrane Image: