Wafer #250409-06 – 1 μm Microslit
Manufacturer’s Data
- Logged by: Ahmet Gurcan
- Membrane Type: MSSN 1 micron Microslit
- SKU: MSSN400.C-3LX.1-1.0E2
- Lot Number: 250409-06
- Quantity Received: 160
- Manufacturer Test Report:
- Flow Data Avg in SLPM
- 4psi: 5.1
- 15psi: 11.87
- Burst: 45.45 PSI
- Flow Data Avg in SLPM