Bonding PDMS to SU-8, from URNano Workshop

This is the method Brian McIntyre developed for the recent URNano Microfluidics Workshop. Based on a polyaddition-based mechanism based on introducing amine groups onto the surface of one material and epoxy groups on another material and enabling the amine–epoxide polyaddition reaction at their closely contacted solid-to-solid interface to establish a covalent and permanent bonding presented in a paper in Polymer, vol 50, issue 23, 3 Nov 2009 pp 5358-61

Screen Shot 2014-07-07 at 1.20.05 PM

The two surfaces, SU-8, and PDMS are modified to facilitate bonding. The SU-8 is ‘modified’ by not hardbaking. This is intended to maximize the dangling surface epoxy chain ends.

With the PDMS, the chain siloxane ends are modified with the addition of N forming amine groups on the surface.

Bringing two sides together at 100º C under clamping pressure for 1hr creates an irreversible bond.

Screen Shot 2014-07-07 at 1.19.26 PM

Screen Shot 2014-07-07 at 1.19.34 PM

 

Screen Shot 2014-07-07 at 1.19.47 PM

Screen Shot 2014-07-07 at 1.19.53 PM

 

Result