Polycarbonate track-etch membrane with high pore length-to-diameter aspect ratio
I would like to share a collection of high resolution SEM images of nanopores of polycarbonate track-etch (PCTE) membrane. These nanopores have very high pore length-to-diameter aspect ratio of 6000 nm / 25 nm. I hope you find them useful.
![]() |
![]() |
![]() |
Cross-section of PCTE membrane
![]() |
![]() |
![]() |
![]() |
Cross-sectional view of long and straight nanopores with a close-up at pore entrance
![]() |
![]() |
![]() |
Cross-sectional view of long and straight nanopores with a close-up at pore entrance










Can you please explain how you did this? Freeze-fracture?