Wafer #240803-17 – 3 μm Dual Scale – Low Porosity
Manufacturer’s Data
- Delivery Date: 12/20/2024 (picked up and logged by Ahmet Gurcan)
- Membrane Type: NPN 3 micron Dual Scale
- SKU: DSSN100-1L-3.0-A1 (0.625% Porosity – Not real porosity)
- Lot Number: 240803-17
- Quantity Received: 320
- Manufacturer Test Report:
- Average Porosity (nanoporosity): 15.1%
- Average Diameter (microporous): 2.898 μm
- Average Diameter (nanoporous): 50 nm
- Average Flux @ 1 PSI: 0.1762
- Average Flex @ 2 PSI: 0.242
- Average Burst Pressure (PSI): 3.768
- Packing slip & invoice: None
UR Testing
- Average Porosity (nanoporosity): 14.39%
- Average Porosity (microporoisty):
- Pore Size (nanopores): 60.14 +/- 18.59 nm
- Pore Size (micropores):
- Pore morphology: Standard
- EDS: N/A
- Chip and Membrane Appearance:
- Window is highly clean. Outside of the window might have some shards from the cutting process and has some white scratches and digs.
- Membrane dimensions (flat surface): 0.7 mm x 2 mm
- Full Test Report / Images in Box: https://rochester.box.com/s/cgxc49oavf8znzpmnp5a1f17wif5djil