Wafer #24240803-19 – 1 Slot NPN
Manufacturer’s Data Delivery Date: 6/3/2024 (picked up and logged by Ahmet Gurcan) Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 24240803-19 Quantity Received: N/A Manufacturer Test Report: Pore Size: 46.5 nm Porosity: 11.3% Flow Data Avg in SLPM 2psi: 0.132 4psi: 0.262 Burst: 5.497 PSI UR Testing Porosity: 11.52% Pore size: 54.25 +/- 15.63…