Wafer Testing: W520, 558, 559
I recently received three pinhole-ridden wafers for cell-related experiments. All three have been RTPed at 800C for 5 minutes in argon, which is the typical procedure we have been using for cell culture. The bursts pressures for each wafer are shown below. W520 is weaker than 558 and 559; I plan on using the stronger…