Update of W637
Dave delivered W637, a wafer made using the sample recipe as W504, to us today. This wafer has a high occurrence of single pinholes, with only 12 samples pinhole-free. I also noticed some odd features on the membranes, shown below.
In the reflection images above, some sort of substance is on the membrane. In the top image it looks like the material has come from the pinhole. All membranes on this wafer have this residue/material; I am unsure what it is. It is not visible in transmission mode.