W613 Discoloration
Given the mixed results of discoloration of RTPed samples from W613, which include no discoloration until 7 days (when the experiment was started within 2 hours of RTPing), and discoloration within 2 days (experiment started 8 days after RTP) I ran another discoloration test. This time I started the experiment within an hour of RTP, and discoloration was seen between 3-5 days. All experiments were run in the same way, except for length of time after RTP to start the experiment. A summary of all three experiments is shown below.