Movable Cutoffs in Diffusion

Follow-up to Pressurized Movable Cutoffs.

Wafers 670 and 673 were not holding up in PBS for the 24 hour diffusion experiment duration.  RTP treatment at 800C for 60s enabled chips from both of these wafers to last 24 hours.  Here are the results from the gels:

We definitely have two different cutoffs in these experiments.  Reduction of small molecular weight species in the retentates is not as extreme as I usually see, but it seems that the porosity on these samples is lower than some of our old membranes.