Synergistic Control of Mesenchymal Stem Cell Differentiation by Nanoscale Surface Geometry and Immobilized Growth Factors on TiO2 Nanotubes

von_der_Mark_2012

Here is some data on cell growth on different porosity TiO2 nanotubes.  The above paper is an earlier publication regarding the work presented in Poster form at PSST 2014.  Below are photos taken from the 4 quadrants of the poster.

cells on nanotubes poster 1
cells on nanotubes poster 1
cells on nanotubes poster 2
cells on nanotubes poster 2
cells on nanotubes poster 3
cells on nanotubes poster 3
cells on nanotubes poster 4
cells on nanotubes poster 4

 

 

 