Wafer #1532 – 2 Slot Wide NPN

Manufacturer’s Data

  • Delivery Date: 3/14/2024 (picked up and logged by Ahmet Gurcan)
  • Membrane Type: 2 Slot NPN – Wide
  • SKU: NPSN100-2LWMS
  • Lot Number: 1532
  • Quantity Received: 299
  • Manufacturer Test Report:
    • Avg Porosity: 13.4%
    • Avg Pore diameter: 48.7nm
    • Avg flux SLPM at 2PSI: 0.244
    • Avg flux SLPM at 4PSI: 0.462
    • Avg Burst Pressure: 6.564
  • Packing slip & invoice: None

 

UR Testing

  • Porosity: 10.9 +/- 1.8 %
  • Pore size: 54.0 +/- 4.3 nm
  • Pore morphology: Standard
  • EDS: N/A
  • Chip and Membrane Appearance:
  • Membrane dimensions (flat surface): 2 x 0.7 mm x 2 mm
  • Representative Membrane Image: See Below

Experiences

  • Cell culture
    • N/A as of 3/14/2024