Paper for Review: Nanoporous Parylene for Ultrafiltration
If you know me at all, you know I enjoy nothing more than ultrafiltration and Parylene-C deposition. Now these activities are combined into one device to improve the biocompatibility (platelet activation and adhesion) of nanoporous membranes. In this letter, polyethersulfone (PES) membranes were coated with Parylene-C, poly(chloro-para-xylylene) aka (PCPX), while glycerin vapors rising through the…