Adsorption Studies
The following changes were made in this adsorption study: The MicroCons/NanoSeps were not spun. We will just characterize the differences between the materials. The pnc-Si membranes were assembled into SepCons because of the potential adsorption to the plastic surfaces. Mass standards were run on the gel in order to allow the measurement of protein concentration….