Wafer #240803-03 – 1 Slot NPN
Manufacturer’s Data Delivery Date: 12/3/2024 (picked up and logged by Ahmet Gurcan) Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240803-03 Quantity Received: 350 Manufacturer Test Report: Pore Size: 16.9% Porosity: 56.4 nm Flow Data Avg in SLPM 2psi: .169 4psi: 0.343 Burst: 3.551 UR Testing Porosity: 13.83% Pore size: 55.6 +/- 14.8 Pore…