Wafer #5241- 0.5 μm Microporous
Manufacturer’s Data Delivery Date: 7/26/2024 (picked up and logged by Ahmet Gurcan) Membrane Type: MPSN 0.5 Microporous SKU: MPSN400.C-3LX.1-0.5L1 Lot Number: 5241 Quantity Received: 180 Manufacturer Test Report: Pore Size: 527.48 nm Flow Data Avg in SLPM 2psi: 2.042 4psi: 4.032 Burst: 29.124 Packing slip & invoice: None UR Testing Pore size: Pore morphology: Smooth…