Skip to content

Nanomembrane Research Group

  • Home
  • Publications
  • MembranesExpand
    • Common Chip Formats
    • Common Membranes
    • Microslit Membranes
  • DevicesExpand
    • µSiMExpand
      • Geometry
      • µSiM CAD Files
      • AssemblyExpand
        • Protocols.io (µSiM Assembly)
        • Instructions
        • Common Issues and Troubleshooting Tips
      • Cell Culture ProtocolsExpand
        • Top Well: hCMEC/D3
        • Top Well: HUVEC
        • Bottom Channel Culturing
        • Immunocytochemistry Protocol
        • Impact of Chip Orientation on Fluorescence Imaging
        • Permeability: In Situ Method
        • Permeability: Sampling Method
        • Cell Culture Common Issues and Troubleshooting Tips
    • SepCon®Expand
      • Sepcon Assembly
      • Sepcon Video Protocol: Assembly
      • SepCon Gasket Silhouette File
      • SepCon Video Protocol: Wetting the membrane
      • SepCon Video Protocol: Disassembly
    • µSiM-DXExpand
      • µSIM Video Protocol: Capture of Nanoparticles
  • ImpactExpand
    • TraCe-bMPS
    • HCIC
    • LOMP
    • SiMPore
Nanomembrane Research Group
  • NRG

    Long Term Urea: Evaporation measurement and Pressure Calculations.

    ByDean Johnson June 13, 2013July 7, 2014

    The initial measurements with multiple tests tubes containing either Serum or PBS failed to demonstrate evaporation and in fact the weights of the collection tubes increased after sitting in the refrigerator overnight. Perhaps the tape collected water? At any rate (<– trite expression), I redid the experiment with a single tube of serum. The tube…

    Read More Long Term Urea: Evaporation measurement and Pressure Calculations.Continue

  • NRG

    Filtration of DNA and Bugs @ INT

    ByJim June 11, 2013

    Two experiments were performed to explore application of SiMPore filters within INT’s microfluidic cartridges to allow the capability for pathogen type specificity in nucleic acid purification. 1) The first experiment tested the efficiency at which nucleic acids could pass through the membranes. T4 polynucleotide kinase was used to 32-P radiolabel two different sized PCR products:…

    Read More Filtration of DNA and Bugs @ INTContinue

  • NRG

    Membrane Permeability Testing

    ByMichael Potter June 10, 2013

    Summary of Results Membrane Pore Diameter Thickness Porosity Permeability (cc/cm^2*min*bar) SiN 3.2-4.0 um 0.12 um 22.1%-35.3% 30000 PCTE 2.4-3.0 um 9 um 11.9%-16.1% 1652 SiN Experimental Design Permeability of the 3 um pore Si Nitride membranes was assessed using the pictured apparatus: Fluid (ultrapure water) was pumped at a constant rate into a pipet whereupon…

    Read More Membrane Permeability TestingContinue

  • NRG

    SEPCON 0.1% SDS pretreatment

    ByJosh Winans June 10, 2013July 7, 2014

    After discussions with the gentleman in charge of surface functionalization at INT last week, Jim suggested that I attempt to pretreat our membranes with 0.1% SDS before a filtration.  The hope being that some surfactant left on the surface of the membrane would be enough to facilitate water passage through the membrane without wetting the…

    Read More SEPCON 0.1% SDS pretreatmentContinue

  • NRG

    MATLAB Installation

    ByJim June 7, 2013July 7, 2014

    Good morning, We received some messages from customer who are having trouble logging into their Matlab account. If you are having trouble accessing Matlab, please see below for your update instructions. If you continue to have Matlab issues, please contact Matlab support at http://www.mathworks.com/support/contact_us/index.html. License number 680214. Your activation Key is:28093-41703-14274-60467-52214. Matlab update instructions: Open…

    Read More MATLAB InstallationContinue

  • NRG

    Attempts in Making PDMS Gaskets in CytoVu Assemblies Play Nicely with PEGylation

    ByTucker Burgin June 7, 2013

    This summer I’ll be working on preliminary development of technology that might lead to SiMPore drug discovery assays. The goal is to use SiMPore membranes to create much more efficient and generalized assays, which represents a big opportunity for the company. However, several challenges need to be addressed in order to make such a device…

    Read More Attempts in Making PDMS Gaskets in CytoVu Assemblies Play Nicely with PEGylationContinue

  • NRG

    Problems with lab door

    ByJim June 6, 2013

    Can someone help explain this e-mail? Hey Jim – Just got a call from the locksmith who had a report from security that someone in your lab is tampering with the lock on your lab door…by doing what they’re doing, they are able to get into your lab without a key (or swiping).  It’s been…

    Read More Problems with lab doorContinue

  • Protocols

    Schematic of Long Term Clearance Test Setup.

    ByDean Johnson June 6, 2013May 21, 2014

    This is the setup used for the long term clearance testing. The fraction collector can be set to advance to the next collection tube at set intervals from 1 min to 99 min. I am currently conducting an evaporation test with both PBS and 100% serum. I weighed six collection tubes, two were filled with…

    Read More Schematic of Long Term Clearance Test Setup.Continue

  • NRG

    Specialized Susceptors for SSI RTP in URnano

    ByJosh Winans June 6, 2013January 23, 2014

    A new user in URnano has used the “old” susceptor for a ~270 C  (I might have the exact number wrong, but it is relatively low temp) to heat In on GaAs.  I don’t think there was ever a good reason for using the RTP for this process, but what is done is done.  I…

    Read More Specialized Susceptors for SSI RTP in URnanoContinue

  • NRG

    PEG Microarray Solution Dilution and X-linker Concentration Study

    ByKate Busse June 4, 2013

    Working on the development of PEG microarrays for cell heterogeneity applications. Current work has been accomplished on TPM coated glass coverslips. Transfer to membranes are in progress. Three different x-linker concentrations were tested in a 1:1 mixture of PEG and DI or PBS. We are testing for what will make the most optimal cell culture…

    Read More PEG Microarray Solution Dilution and X-linker Concentration StudyContinue

Page navigation

Previous PagePrevious 1 … 117 118 119 120 121 … 231 Next PageNext

© 2026 Nanomembrane Research Group - WordPress Theme by Kadence WP

0
    0
    Your Cart
    Your cart is emptyReturn to Shop
    Continue Shopping
    • Home
    • Publications
    • Membranes
      • Common Chip Formats
      • Common Membranes
      • Microslit Membranes
    • Devices
      • µSiM
        • Geometry
        • µSiM CAD Files
        • Assembly
          • Protocols.io (µSiM Assembly)
          • Instructions
          • Common Issues and Troubleshooting Tips
        • Cell Culture Protocols
          • Top Well: hCMEC/D3
          • Top Well: HUVEC
          • Bottom Channel Culturing
          • Immunocytochemistry Protocol
          • Impact of Chip Orientation on Fluorescence Imaging
          • Permeability: In Situ Method
          • Permeability: Sampling Method
          • Cell Culture Common Issues and Troubleshooting Tips
      • SepCon®
        • Sepcon Assembly
        • Sepcon Video Protocol: Assembly
        • SepCon Gasket Silhouette File
        • SepCon Video Protocol: Wetting the membrane
        • SepCon Video Protocol: Disassembly
      • µSiM-DX
        • µSIM Video Protocol: Capture of Nanoparticles
    • Impact
      • TraCe-bMPS
      • HCIC
      • LOMP
      • SiMPore