Skip to content

Nanomembrane Research Group

  • Home
  • Publications
  • MembranesExpand
    • Common Chip Formats
    • Common Membranes
    • Microslit Membranes
  • DevicesExpand
    • µSiMExpand
      • Geometry
      • µSiM CAD Files
      • AssemblyExpand
        • Protocols.io (µSiM Assembly)
        • Instructions
        • Common Issues and Troubleshooting Tips
      • Cell Culture ProtocolsExpand
        • Top Well: hCMEC/D3
        • Top Well: HUVEC
        • Bottom Channel Culturing
        • Immunocytochemistry Protocol
        • Impact of Chip Orientation on Fluorescence Imaging
        • Permeability: In Situ Method
        • Permeability: Sampling Method
        • Cell Culture Common Issues and Troubleshooting Tips
    • SepCon®Expand
      • Sepcon Assembly
      • Sepcon Video Protocol: Assembly
      • SepCon Gasket Silhouette File
      • SepCon Video Protocol: Wetting the membrane
      • SepCon Video Protocol: Disassembly
    • µSiM-DXExpand
      • µSIM Video Protocol: Capture of Nanoparticles
  • ImpactExpand
    • TraCe-bMPS
    • HCIC
    • LOMP
    • SiMPore
Nanomembrane Research Group
  • NRG

    Adsorption Quantification IV

    ByJessica Snyder June 16, 2008

    Previously we have worried about the validity of our adsorption data considering we have used it to test both sides of anisotropic membranes that have cutoffs below the size of albumin. Today we came up with the idea that albumin can be used as a probe for adsorption, not as simply a model protein in…

    Read More Adsorption Quantification IVContinue

  • NRG

    HUVEC Adhesion with Controls

    ByKarl Reisig June 16, 2008

    HUVEC adhesion was measured on glass, tissue culture plastic, and pnc-Si, with poly-lysine coated plastic and teflon coverslips as positive and negative controls. Adhesion on pnc-Si was low, this could be due to cells being lost through broken slits or possibly some other unknown factor. Adhesion tests are continuing, with the use of solid Si…

    Read More HUVEC Adhesion with ControlsContinue

  • NRG

    Micropump Update

    ByMike H June 16, 2008

    Finally on Friday all the pieces came in that we ordered to connect the peristaltic pump tubing to the 238umOD capillary tubing. This is our first order, after last weeks meeting we ordered a smaller OD capillary tubing (164um) with the same 100umID. I connected all the pieces and attached the micropump to make sure…

    Read More Micropump UpdateContinue

  • NRG

    Adsorption Quantification III

    ByJessica Snyder June 15, 2008

    UPDATE: Teflon data now include Original Post: Refer back to Part I, and Part II This weekend I ran a bunch of gels to flesh out the adsorption data a bit more. I tested MicroCons, NanoSeps, and teflon and reran the initial Pnc-Si gel to get rid of negative results due to uneven staining. To…

    Read More Adsorption Quantification IIIContinue

  • NRG

    pinhole-less membranes

    ByDave Fang June 13, 2008

    Inspired by JP, we decided to try to etch amorphous (unannealed) wafers this week to see if pinhole density changed.  To my surprise, the amorphous membranes had no pinholes!  Furthermore, I tried to anneal the membranes after the etch and they went flat indicating crystallization!  Refer to the table below for the results. Wafer 565:…

    Read More pinhole-less membranesContinue

  • NRG

    COMSOL modeling progress…

    ByMike H June 13, 2008

    Over the last few days I have spent some time learning the basics of the COMSOL modeling software. I have just started to understand the basics and I just wanted to show an example of what this program is capable of. Below are images of flow modeled through a  “non-uniform pore”. This model assumes water…

    Read More COMSOL modeling progress…Continue

  • NRG

    Fibroblast adhesion study using controls

    ByAnant Agrawal June 13, 2008

    Fibroblast adhesion experiment was done using poly-lysine coated plastic and teflon coverslips as positive and negative controls repectively. Poly-lysine is a polypeptide that gives the cells a sticky surface to adhere to. Teflon coverslips are used as negative control because they do not promote cell adhesion. Difference in morphology of cells could also be seen…

    Read More Fibroblast adhesion study using controlsContinue

  • NRG

    Polycarbonate Sheet — substrate material

    ByJim June 11, 2008

    I worked with Paul this afternoon and finally we highly suspect the raw material used for the prototype diffusion chamber could be Polycarbonate. Paul could not provide direct evidence for the material source since he did not keep any purchase orders or materials data sheet… However, we did check our chamber with another plastic board…

    Read More Polycarbonate Sheet — substrate materialContinue

  • NRG

    Question about observation through the plastic substrate of the new diffusion chamber

    ByJim June 11, 2008

    Attached are the photos taken under DIC and Rhodamine channels, using the new diffusion chamber. I can clearly observe Rhodamine pass to the lower hole of the chamber, under the Rhodamine channel by eye ball. But from what I got using the Matlab software, it looks weird because both DIC and Rhodamine photos look very…

    Read More Question about observation through the plastic substrate of the new diffusion chamberContinue

  • NRG

    Worth a read

    ByDave Fang June 11, 2008

    fornasiero2008

    Read More Worth a readContinue

Page navigation

Previous PagePrevious 1 … 208 209 210 211 212 … 231 Next PageNext

© 2026 Nanomembrane Research Group - WordPress Theme by Kadence WP

0
    0
    Your Cart
    Your cart is emptyReturn to Shop
    Continue Shopping
    • Home
    • Publications
    • Membranes
      • Common Chip Formats
      • Common Membranes
      • Microslit Membranes
    • Devices
      • µSiM
        • Geometry
        • µSiM CAD Files
        • Assembly
          • Protocols.io (µSiM Assembly)
          • Instructions
          • Common Issues and Troubleshooting Tips
        • Cell Culture Protocols
          • Top Well: hCMEC/D3
          • Top Well: HUVEC
          • Bottom Channel Culturing
          • Immunocytochemistry Protocol
          • Impact of Chip Orientation on Fluorescence Imaging
          • Permeability: In Situ Method
          • Permeability: Sampling Method
          • Cell Culture Common Issues and Troubleshooting Tips
      • SepCon®
        • Sepcon Assembly
        • Sepcon Video Protocol: Assembly
        • SepCon Gasket Silhouette File
        • SepCon Video Protocol: Wetting the membrane
        • SepCon Video Protocol: Disassembly
      • µSiM-DX
        • µSIM Video Protocol: Capture of Nanoparticles
    • Impact
      • TraCe-bMPS
      • HCIC
      • LOMP
      • SiMPore