Krishanu Shome's Thesis Defense

The Institute of Optics, University of Rochester University of Rochester, Rochester, NY Ph.D. Public Defense

Interaction of Light with Metallized Ultrathin Silicon Membrane

Krishanu Shome
Advisor: Professor Philippe M. Fauchet

Wednesday, February 27, 2013 Time 9:00 a.m. Place Wilmot 116

Freestanding metallized structures, a few tens of nanometer thick, show promise in creating flow-through sensors, single molecule detectors and novel solar cells. In this thesis we study test structures that are a step towards creating such devices. Finite- difference time-domain simulations have been used to understand and predict the interaction of light with such devices. Porous nanocrystalline silicon membrane is a novel freestanding layer structure that has been used as a platform to fabricate and study sensors and novel slot nanohole devices. Optical mode studies of the sensing structures, together with the method of fabrication inspired the creation of ultrathin freestanding hydrogenated amorphous silicon p-i-n junctions solar cells. All the freestanding structures used in this thesis are just a few tens of nanometers in thicknesses.

In the first part of the thesis the sensing properties of the metallized porous nanocrystalline structure are studied. The surprising blueshift associated with the sensing peak is observed experimentally and predicted theoretically with the help of simulations. Polarization dependence of the membranes is predicted and confirmed for angled deposition of metal on the membranes.

In the next part, a novel slot structure is fabricated and modeled to study the slot effect in nanohole metal-insulator-metal structures. Atomic layer deposition of alumina is used to conformally deposit alumina within the nanohole to create the slot structure. Simulation models were used to calculate the lowest modal volume of 4×10-5 μm3 for an optimized structure.
In the last part of the thesis, freestanding solar cells are fabricated by effectively replacing the porous nanocrystalline silicon layer of the membranes with a hydrogenated amorphous silicon p-i-n junction with metal layers on both sides of the p-i-n junction. The metal layers act both as electrical contacts as well as mirrors for a Fabry Perot cavity resonator. This helps in tuning the absorption profile of the solar cell to target near infrared part of the solar spectrum. A correspondence is found between the simulation absorption results with the experimental spectral response of the solar cells. This helps in designing metallized solar cells with ITO layer to improve absorption and hence the efficiency.