RTP Ramp Rate Effect on 6W Bias pnc-Si Stack Increases Pores Size Slightly
Purpose: We want to know the effects of the RTP process on pore size, pore density for the biased films coming out of the AJA. I believe that the RTP ramp rate is important for forming bigger pores. Some work (Joe Qi Thesis) has indicated that the pores come out more circular as the wafer is…
8 hour diffusion
Because of the recent discoloration problems I observed with 24 hour diffusion using w670 and 673, I decided to try a shorter time point. 673 had a couple more samples to spare, so I tried an 8 hour diffusion experiment. No discoloration was observed: This is the normal color of the wafer. Slits were not…
Bottom SiO2 Thickness Experiment(1)
ByJoe QiThe thickness of bottom oxide in the ‘sandwich structure’ is also a key factor to affect the pore morphology. In last few weeks I deposited five wafers with different bottom oxide thicknesses and they were 05/15/20, 10/15/20, 20/15/20, 40/15/20 and 100/15/20. Then I annealed them at 1000C for 1 minute with a 100C/s ramp rate….
Life Expectancy Trend of ESRD Patients Treated with Dialysis (1995-2013)
Introduction Over the past two decades there has been little to no improvement in treatment for people who have end stage renal disease (ESRD). The two main methods of treatment for ESRD are kidney transplant or dialysis. However, due to the limitations involved with transplantation, the majority of patients receive dialysis. It has been speculated…
The Big Squeeze: Unintentionally Pulling Staphylococcus aureus Through 0.5 µm Microporous Membranes
On our quest to improve the performance of bacterial assays that use the µSiM-CA by modifying our standardized protocol, our most recent modification has caused controversy. Described here, we recently decided to add a step to our protocol where we pull fluorescently tagged Staphylococcus aureus onto the membrane by withdrawing a bacteria filled solution which we load…