Wafer #240919-17 – 1 Slot NPN
Manufacturer’s Data
- Delivery Date: 4/28/2025 (picked up and logged by Ahmet Gurcan)
- Membrane Type: NPN 1 Slot
- SKU: NPSN100.C-1LZ.0
- Lot Number: 240919-17
- Quantity Received: 360
- Manufacturer Test Report:
- Pore Size: 63.2 nm
- Porosity: 17.1%
- Flow Data Avg in SLPM
- 2psi: 0.08
- 4psi: 0.169
- Burst: 6.781 PSI
UR Testing
- Porosity: 8.19%
- Pore size: 55.33 +/- 14.11 nm
- Pore morphology: Standard
- EDS: N/A
- 3 Membranes from this lot were removed for QC measurements.
- Membrane dimensions (flat surface): 0.7 mm x 2 mm
- For more information visit: https://rochester.box.com/s/dmbp9aqo6958r0bzl59mxsd3igwbiq89