Macro To Represent Wafer Characterization
Charles designed a macro for excel to represent the data gathered from wafer characterization, in a visual format. It is built on VB platform and runs off Microsoft excel. The data is input in a simple fashion by selecting the relevant field from a drop down box for columns representing different positions (see fig. 1)….
Cytotoxicity of silver chloride and platinum electrodes
I am working with different electrode materials as a substitute for ITO for my TEER measurement device. I used silver-silver chloride electrode and platinum-iridium ribbon (90:10) for that purpose. I made AgCl electrode by dipping about an inch of silver wire in silver chloride ink and letting it dry for half hour. I obtained the…
Designing a two-channel 6-plex μSiM platform
BypmiltonOverview The main aim of my rotation in the McGrath lab was to design a new 6-plex two-channel μSiM platform. Currently, individual two-channel μSiM platforms are used for tissue-on-a-chip experiments. Expanding the current two-channel single (1-plex) platform to a two-channel 6-plex setup will increase experiment throughput and efficiency, as well as provide a starting point…
BMES 2014 Talk Comments – Greg
Here are my thoughts on the talks I attended at BMES: OP-Thurs-1-11. BioMEMS I Oral Thursday, October 23, 2014 8:00 AM – 9:30 AM Room 008A Moderator 1: James Tunnell Moderator 2: Catherine Klapperich 8:15 AM – 8:45 AM High-throughput High-content Developmental Biology and Neurogenetics H. Lu. Abstract This talk used a number of image processing…
Resistance comparison
In this post I look at our membrane resistance and compare it to the best performing alumina membrane. Here is the resistance figure I made for the paper: This figure shows the device resistance with and without a membrane. The membrane resistance would be the difference between the white and grey bars. We would like…
Carbonization can occlude pores
Last week I reported that carbonization can shrink pores. This week I was able to completely occlude the pores with a change in the process recipe. Instead of cutting off the acetylene flow before the thermal treatment, I kept the gas on for the entire process. What resulted was a complete occlusion of the pores….