Wafer #251028-02 – 0.5 μm Microslit
Manufacturer’s Data
- Logged by: Ahmet Gurcan
- Membrane Type: MSSN 0.5 micron Microslit
- SKU: MSSN400.C-3LX.1-0.5E1
- Lot Number: 251028-02
- Quantity Received: 250
- Manufacturer Test Report:
- Flow Data Avg in SLPM
- 4psi: 3.88
- 15psi: N/A
- Burst: 9.22 PSI
- Flow Data Avg in SLPM