Wafer #240803-12 – 1 Slot NPN
Manufacturer’s Data Delivery Date: 12/18/2024 (picked up and logged by Ahmet Gurcan) Membrane Type: NPN 1 Slot SKU: NPSN100.C-1LZ.0 Lot Number: 240803-12 Quantity Received: 320 Manufacturer Test Report: Pore Size: 50.5 nm Porosity: 11.6 Flow Data Avg in SLPM 2psi: 0.16 4psi: 0.307 Burst: 4.919 UR Testing Porosity: 9.99% Pore size: 50.62 +/- 14.61 nm…