FISHER team and PETL instructions

Hi all, just a quick posting to update you and deposit the current SOP and video instructions for PETLs.

Nick has been working this summer on culturing cells on PETLs; its been slow, but we are finding that cells (HEKs) are happy growing on curated (cooked) EVA, not so much on the PET side. Right now we are working on evaporation issues and reservoirs.

Please check this link if you are interested in watching the process of building PETLs.  I attach here the SOP pdf.

Cheers,

Fernando

PETL_SOP_2016

Video:  https://www.youtube.com/audio?v=bq63xrQBaA8