Wafer #1531 – 3 micron Dual Scale – High Porosity

Manufacturer’s Data

  • Delivery Date: 3/14/2024 (picked up and logged by Ahmet Gurcan)
  • Membrane Type:  NPN 3 micron Dual Scale High Porosity
  • SKU: DSSN100-1L-10%-3.0
  • Lot Number: 1531
  • Quantity Received: 315
  • Manufacturer Test Report:
    Avg Porosity: 15.1%
    Avg Nano Pore diameter:50.7nm
    Avg Micro Pore diameter: 2.986um
    Avg flux SLPM at 1PSI: 0.445
    Avg flux SLPM at 2PSI: 0.720
    Avg Burst Pressure: 3.493
  • Packing slip & invoice: None