Burst Pressures and Air Permeability after Ozone treatment

I tested ozone treatment influence on the membrane strength and air permeability. The result: didn’t see any difference between ozone treated and non-treated samples.

Burst pressure experiments description: tried wafers 391, 393, 344, and 345. Ozone treatment for 5 and 15 min didn’t show any difference.

Air permeability: tested samples from wafers 344, 345 with different porosities before treatment and after.