The Long Road to Wearable Dialysis
Directory containing article and presentation Nature Article about Willem Kolff
Directory containing article and presentation Nature Article about Willem Kolff
Theoretical molar flow is calculated for membranes with different porosities and is based on data extracted from TEM images using Mike’s program. Experimental data is calculated using air permeability test results. It is associated with porosity only through TEM data. Correlation between two is very good but some points do not agree. One of the…
I figured I’d throw this up in case anyone needed to know how to order anything… enjoy. http://docs.google.com/Presentation?id=ddfnw7hd_235d2f4v4f5
I have uploaded the TEOS process outline: TEOS is tetra-ethyl-ortho-silicate, or equivalently tetra-ethoxy-silane. TEOS slowly hydrolyzes into silicon dioxide and ethanol when in contact with ambient moisture. IMPROVEMENTS: -This process prevents us from having to expose the front-side of the silicon during processing. Concurrently, this eliminates the need for aggressive cleaning of the front surface…
Production was scarce last week because we ran into some problems with our patterning/etch process. The first two wafers I attempted to etch did not react with the EDP because there was a thicker than normal layer of oxide remaining after our lithography step which prevented the EDP from attacking the underlying bulk silicon. We’ve…
I measured burst pressures on two non-unifrom wafers w391, w393. They have lots of pinholes (especially w391) but the pressure they withstand is pretty high. I expected it to be much lower after looking at the membranes in the microscope.
Attached is a series of images we took of two populations of neutrophils above and below the membrane.I’m including by methodology for those who are interested:One population was pre-labeled with AF488 (green) antibody against L-selectin, the other with AF546 (red). The green population was suspended in a low protein buffer (~1% serum) and a 20…
A couple of summers ago a Penn State summer student named Joe Fantuzo was working in the lab measuring cell growth rates and cell spreading on pnc-Si membranes and comparing the results to glass coverslips and tissue culture grade plastic. At least that is what we hired him to do. Joe spent much of that…
20nm polystrene beads in 1x PBS passed through w218. This wafer looks a little strange, like it was not fully etched (Dave do you know what happened to this one?). This was just a first stab at the benchtop diffusion with PS, so I didn’t use a “good” membrane. At any rate, the PS went…
Earlier in the week I retested the 100K microcons in our wet-wet EQ format. When I last ran them this way I calculated very little flow and very small permeability values. I noted that there was a rather large air pocket collecting on the underside of the membrane in the plastic support structure; most likely…