Aggregation of 20 nm NPs, IgG, and Tween 20
We had previously tested different surfactants to see if we could get 20 nm polystyrene beads and IgG to stay in suspension while filtering with the centrifuge. We found 0.1% Tween 20 to be sufficient when dealing with 10:1 (5×10^14) 20 nm NPs and 1mg/ml IgG. During the reverse centrifuge studies we mixed 10^15 particles/ml…