5 μm Dual Scale In-Stock
This post is the TraCe and NRG network, letting you guys know that the 5 μm Dual Scale is in stock. They can be checked out by following this link to order from the TraCe-bMPS website and this link to order them from the NRG site.
Below are some SEM images of the 5 μm pores.

Figure 1: a) 37x SEM image of the entire membrane window, b) zoomed in SEM image of individual pores, c) individual pore with sizing data to confirm 5 micron pore size, d) EDAX spectrum data showing detected elements. Mg levels below the generally accepted”true” threshold and Au is present due to the chip being coated in Au for SEM imaging.