Integration of in situ Heating for Microplastic Melting Assay on Silicon Nanomembranes
Document: Ian’s Presentation Thanks to Ian Krout for the experiment and the writeup, which I have organized here. The purpose of this set-up was to develop a tool to melt plastic particles collected on the silicon nanomembranes membranes. Due to the different melting temperatures of plastic polymers this tool allows users the ability to rapidly…