Specialized Susceptors for SSI RTP in URnano
A new user in URnano has used the “old” susceptor for a ~270 C (I might have the exact number wrong, but it is relatively low temp) to heat In on GaAs. I don’t think there was ever a good reason for using the RTP for this process, but what is done is done. I…