Shadow-Masking Microporous and Nanoporous Materials with Silicon Nanomembranes
Summary: The fabrication of NPN relies on the formation of pnc-Si over a non-porous SiN film, then etching the pattern of the pnc-Si into the SiN. I used the same concept to replicate the dual-scale nanomembrane style (microporous+nanoporous) featured in Alec’s work, as well as create a porous/nonporous nanomembrane substrate, by using existing SiN or…