PLL-g-PEG patterning on SiO2 layer
As part of my thesis, I am trying to get a non-fouling pattern on a substrate which resembles our porous membranes to investigate cell behavior including cell adhesion and migration and to compare with our previous results which was obtained on porous membranes. This study can separate the role of pore edges and disrupted surface…