Separation of Microbeads from Whole Blood on 8 and 9 Micron Slit Membranes
A few weeks ago, Josh and JP brought me some 3 window microslit membranes that had edge aligned 8 and 9 μm slits. While these may seem to be quite large for most applications, they are in fact perfect for working with whole blood. The experiments that we have planned for these membranes are based on the…